Moisture Content and Drying of Wood
Wood shrinks and swells twice as much in the direction parallel to the growth rings as it does perpendicular to them. The combined effect of different rates of movement is the cause of warping and twisting. In other words, the growth rings try to straighten out from wet to dry.
Dryer wood will move in the opposite direction when it gains moisture. Wood is only as dry as the air which surrounds it and once dried, it does not always stay that way. Wood will always seek its equilibrium moisture content (EMC) with its environment. No matter how long wood has been seasoned or kiln-dried, its cells still contain some amount of moisture. This is called moisture content (MC). Moisture content changes as the relative humidity (RH) of the air around the wood changes.
Wood is worked in its dry state for various reasons. When dry, wood’s dimensional stability is increased and weight is reduced from the loss of water. Dry wood is not susceptible to decay or rot. When wood is dried, it can greatly increase its strength up to 50% from its original green state.
Kiln drying is a process of seasoning lumber done with high-temperature, steam-heated heat exchanges to control temperature, humidity, and air circulation to dry wood uniformly down to a predetermined MC for each different species.
Typically, this process kills all fungi and insects as well as minimizing dimensional changes in its process. Kiln drying reduces the likelihood of mold, stain, or decay while improving finishing characteristics and machining, screwing, or gluing qualities.
Air drying is a low-cost, low-tech way to dry lumber. This process requires time, effort, and room for stacking or storing. Depending on thickness and width, the process of air-drying lumber may not dry the lumber to less than 15-20% MC.
Staining or mold may occur during the process with little control over drying rates. Wood can become discolored by ultraviolet light and when exposed to air will become dull looking and darker, and is more subject to fungal decay.
Decay is frequently present in living trees and lumber will contain organisms that will continue to develop as it is air-dried. In all stages of air drying, wood can be subject to attack by insects such as powder post beetles. Geographic locations can also vary drying times.
The western red cedar that we predominantly use for the manufacturing of our shutters and blinds arrives at our plant kiln dried with an MC between 8-12% which is optimum for machining, gluing, and stability. We routinely check every unit with an electronic moisture meter to ensure proper moisture levels.
When we use hardwoods such as mahogany, Spanish cedar, or cypress, MC can vary depending on the type. True mahoganies imported from the West Indies, Mexico, and South and Central America will be kiln-dried and further air-dried to 8% MC because of its density and/or from the overseas transportation accepting moisture during the process.
Cypress is much different than most other species, and when kiln-dried, careful attention needs to be used not to over or under dry the wood which can cause pitch pockets or splitting. The typical MC for cypress is 11-14%. Further drying can cause face cracking. When a customer commissions us to replicate shutters or blinds from cypress lumber, we only purchase from a proven, reputable dealer who has a great track record for uniform drying.
This is important because when wood increases its moisture content, it has movement. The seasonal changes in humidity can affect exterior blinds and shutters even when painted and finished. Wood will gain or lose moisture causing expansion and contraction based on its surrounding environments.
An excessive MC, regardless of how it was obtained, either by using sapwood, improper drying procedures, or through improper storage will cause movement in service resulting in malfunctions in joinery. Excessive moisture may create issues with warpage, bowing, rot, cracks, and even paint peeling issues.